Epoxy Priming below the water line on Abandoned Project Catamaran E109
The epoxy priming process begins. First mist coat diluted with 20 percent thinner as prescribed by Hempel for the first mist coat. Makes a visual difference and also highlights the areas that require my attention. Next video should cover the 5 percent dilute coat of Hempel 2k Light primer before i can start fairing and addressing any highlighted issues. The Amazon Wish list is now live here! https://www.amazon.co.uk/hz/wishlist/ls/32HP67P3CCKAZ?ref_=wl_share If you can support my project then please see the links below: https://www.buymeacoffee.com/SailingFoxyLady Fieldy1978@hotmail.com Insta: https://www.instagram.com/sailingfoxyladycatamaran/ facebook: https://www.facebook.com/spencer.field.3/ Teespring: https://my-store-11749339.creator-spring.com/ Patreon: https://www.patreon.com/sailingfoxylady?fan_landing=true Fair Winds and Calm Seas, Spence.